Then the metals are alloyed in oil - fired or electric arc furnaces, and cast into ingots 40 cm wide, 15 cm thick and 6 m long. These ingots are reheated until the temperature is hot enough for hot rolling. During this stage, the ingots pass through a series of rollers until they form long, thin sheets which are the thickness of a coin. From these thin strips, blank discs are punched.